Thank you for a clinically useful presentation.
The chairman has a couple of questions.
1. Comparing GIGAUSS C and D, which factor is supposed to be affecting the magnetic flax leakage, the shape or the size of the magnetic assembly?
2. If you measure C800 and C1000, do you prospect the same tendency with D800 and D1000 or not?
Thank you for your cooperation.
Thank you for your questions.
1.We think both the shape and the size of magnetic assembly will affect. However, we need to examine it with magnetic field analysis( FEM etc).
2.We are not sure, because there are no C800 and C1000 as a product. However, as a prediction, results similar to D800 and D1000 will be obtained.